How to succeed with your SU-8 photoresist UV exposure?
At a glance
SU-8 photoresist UV exposure activates the PAC in selected regions to initiate cross-linking, followed by baking and development. Successful exposure depends on close contact between photomask and resist, relative humidity, bake times and exposure time. Development checks, microscopy and thickness measurements help assess the resulting SU-8 pattern.
- Exposure wavelength
- UV light at 365nm
- Relative humidity
- Exposure not recommended above 70% relative humidity
- Edge bead removal
- Cut out: removing resin on about half a centimeter at the wafer edge with a thin acetone jet
- Exposure time
- Too short: resist may lift off in development; too long: channel width can increase
The SU-8 photoresist UV exposure